Composition

Polyacrylate solution containing amino groups.

 

Typical Properties:

Amine value: 26-30 mg KOH/g

Density: 0.9520°C g/m

Effective content: 100%

Solvent: Butyl acetate

  • Product Details
  • Packing & instructions
  • HH-2016D Solvent-based dispersant

It is a wetting and dispersing aid for solvent-based coatings, used to disperse organic pigments, inorganic pigments and carbon black in organic solvent media. It can improve pigment wettability, reduce the time required for the grinding process and stabilize pigment dispersions.

It deflocculates the pigment through the steric hindrance of the polyacrylate chain and prevents pigment flocculation and precipitation during storage. Since the deflocculated pigment particles are very small, high gloss and enhanced color strength can be obtained.

In addition, transparency and hiding power are increased. These products can reduce the viscosity of the system, thereby improving the leveling of the product and increasing the pigment content.

 

  • Product Data

Composition

Polyacrylate solution containing amino groups.

 

Typical Properties:

Amine value: 26-30 mg KOH/g

Density: 0.9520°C g/m

Effective content: 100%

Solvent: Butyl acetate

Type:HH2016D

*.The values indicated in this data sheet describe typical properties and do not constitute specification limits.

 

  • Applications

Special Features and Benefits

1、Improves the wettability of the pigment, reduces the time required for the grinding process, improves the gloss and leveling, reduces the viscosity and avoids thixotropy.

2、Prevents the re-flocculation of the pigment through the steric stabilization of the polyacrylate chain in the block polymer, so that the tinting power and hue of the pigment in the coating and pigment paste can be stabilized, preventing the flocculation and precipitation of the pigment during storage, and keeping the pigments and fillers in the system evenly dispersed.

3、Since the dispersant has a high molecular weight and similar properties to the resin, it will not affect the durability of the coating base material.

Note: This instruction manual is for reference only and does not have any guarantee properties. Please test its applicability in advance.

 

  • Recommended Use

Used in industrial printing coatings, architectural coatings, coil coatings, automotive coatings, wood and furniture coatings, anti-corrosion coatings, pigment concentrates and other systems.

 

Addition amount

Recommended Levels:

Organic pigments: 10~20

Titanium dioxide: 2-5

Carbon black: 20~30

Inorganic pigments: 2-10

*.Please do a step experiment for the specific amount of addition, the above dosage depends largely on the particle size and specific surface area of  the pigment.

 

Instructions for use

To achieve the best performance, the additives should be added to the grind first, followed by the pigment. Premix the resin and solvent components of the grind, then slowly add the additives while stirring. Do not add the pigment until the additives are well mixed.

All of our dispersants are packaged in export plastic barrels. The main plastic barrel packaging specifications are: 25kg, 125kg, 200kg, 1000kg.

Dispersant Packaging Specifications

Dispersant Packaging Specifications

We also accept customized dispersants and other products. Welcome to contact us!

The information herein is based on our present knowledge and experience.The information merely describes the properties of our products but no guarantee of properties in the legal sense shall be implied. We recommend testing our products as to their suitability for your envisaged purpose prior to use. No warranties of any kind, either express or implied, including warranties of merchantability or fitness for a particular purpose, are made regarding any products mentioned herein and data or information set forth, or that such products, data or information may be used without infringing intellectual property rights of third parties. We reserve the right to make any changes according to technological progress or further developments.

Prev:

Next:

Leave a Reply

Leave a message